HUAYU ADDITIVE 75MnF/ 80MnF /75MnAl/ 80MnAl
Description
Dark gray tablet additive.
Availability
To adjust and compound the content of Mn in aluminum alloys and to replace Al-Mn alloy.
Instruction
When the temperature of melt reaches 730-760¡æ, skim the slag off, add demanded additive,
wait for 10 minutes and stir completely.(If the melt is dirty, should refine again and
deslag, and then add the additive to improve the recovery.)
Application Rate
Added volume=
Needed volume in Al alloys
75%(80%)¡Á90%(recovery percentage)
Note: the recovery of 75MnAl or 80MnAl can reach 95%.
HUAYU ADDITIVE 75 MnF/ 80MnF /75MnAl /80MnAl
•Easy for operation to reduce labor intensity
•it can avoid the oxide and the salt inclusion can purify the melt
•MnAl additive is a high grade product with the special feature of quick melting speed and
high recovery.
Packing
g/tablet Tablets/alum. Foil roll Kg/ alum. Foil roll Kg/carton
200 5 1.00 20.00
500 4 2.00 20.00
1000 2 2.00 20.00
1250 3 3.75 22.50
Note: We can produce and pack according to each customer¡¯s requirements.
Storage
Store in dry warehouse. Avoid absorbing water.
Valid Date: 3 months.
Material Safety Data:
Appearance: dark gray tablet
Density: >4.7g/cm3
Color code label: grey